Thermal storage bricks have brought people a guarantee of safety in the field of safety. The price of magnesia chrome bricks will also cause partial damage to some thermal storage bricks due to external conditions. Then we need to maintain and repair these Thermal storage bricks. The following heat storage bricks will introduce you to the matters needing attention in repairing bricks:


1. The repairing bricks must use the same batch of bricks from the same heat storage brick manufacturer as the old bricks;


2. As far as possible, use the remaining loose bricks repaired at the same time as the old bricks (note: bricks that are damp or damaged are strictly prohibited)


3. The contact surface of new and old bricks must be fired mud;


4. No iron plate can be struck between the new and old brick interface surfaces;

钢包镁钙砖.jpg

5. The joints between the two sides of the lock brick can not be ironed, the iron plates of two adjacent ring bricks should be staggered, and the two sides of the same brick cannot be ironed;


6. The iron plate must be completely driven into the brick gap;


7. The sealing of the first few rings of bricks must be inserted from the side, and the last ring of bricks should be sealed with front inserts;


8. Carry out masonry in strict accordance with the design brick ratio, and do not change the masonry ratio at will;


9. The cardboard for the expansion joints of the dug bricks must not be torn off, and the dug bricks must be wet-laid (the fullness of the fire mud should be more than 95%. It is strictly forbidden that the big end of the brick has no fire mud and the small end has fire mud. If this happens, it should be Dismantle and rebuild in time;


10. Do not use (or reduce the use) of processed bricks when digging and repairing. 